Chemical composition:
Executive |
Classification |
Alloy |
Cu |
Al |
Fe |
Mn |
Ni |
P |
Pb |
Si |
Sn |
Zn |
Total amount of |
ISO24373 |
Cu6338 |
CuMn13Al8Fe3Ni2 |
bal. |
7.0-8.5 |
2.0-4.0 |
11.0-14.0 |
1.5-3.0 |
- |
0.02 |
0.1 |
- |
0.15 |
0.5 |
GB/T9460 |
SCu6338 |
CuMn13Al8Fe3Ni2 |
bal. |
7.0-8.5 |
2.0-4.0 |
11.0-14.0 |
1.5-3.0 |
- |
max0.02 |
max0.1 |
- |
max0.15 |
max0.5 |
BS EN14640 |
Cu6338 |
CuMn13Al7 |
bal. |
6.5-8.5 |
1.5-4.0 |
11.0-14.0 |
1.5-3.0 |
- |
0.02 |
0.1 |
- |
0.15 |
0.5 |
AWS A5.7 |
C63380 |
ERCuMnNiAl |
bal. |
7.0-8.5 |
2.0-4.0 |
11.0-14.0 |
1.5-3.0 |
- |
0.02 |
0.1 |
- |
0.15 |
0.5 |
DIN 1733 |
2.1367 |
SG-CuMn13Al7 |
bal. |
6.5-8.5 |
1.5-3.0 |
11.0-14.0 |
1.5-3.0 |
- |
max 0.02 |
max0.1 |
- |
max0.15 |
max0.4 |
Physical properties of materials:
Density |
Kg/m3 |
7.4 |
Melting range |
ºC |
945-985 |
Thermal conductivity |
W/m.K |
30 |
Electrical conductivity |
S.m/mm² |
3-5 |
Coefficient of thermal expansion |
10-6/K(20-300ºC) |
21.5 |
Standard values of the weld metal:
Elongation |
% |
10 |
Tensile strength |
N/mm2 |
900 |
Notched bar impact work |
J |
180 |
Brinell hardness |
HB 2.5/62.5 |
290 |
Particularly suitable for highly stressed corrosion resistant overylay welding on cast iron and on unalloyed and low alloyed steels.Seawater resistant zinc free copper aluminium manganese alloy with high tensile strength and hardness.
Make up:
Diameter:1.20 - 1.60 -2.0-2.40
Spools:D100,D200,D300,K300,KS300,BS300
Rods:1.20 - 4.0 mm x 350mm-1000 mm
Further make ups on request