Customization: | Available |
---|---|
Type: | Copper Wire |
Application: | Resistance |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Main chemical composition :
Alloy type |
Cu |
Mn |
Ni |
6J8 |
rest |
8-10 |
/ |
6J12 |
rest |
11-13 |
2-3 |
6J13 |
rest |
11-13 |
2-5 |
Related parements of Manganin wire:
Item |
6J8 |
6J12 |
6J13 |
Resistivity |
0.35±0.05 |
0.47±0.03 |
0.44±0.04 |
TCRx10-6/°c |
-5~+10 |
-10~+20 |
0~40 |
EMF V S Cu(0-100°c)uv/°c |
≤2 |
≤1 |
≤2 |
Density(g/cm3) |
8.7 |
8.4 |
8.4 |
Melting point (°c) |
960 |
960 |
960 |
Tensile strength(MPa) |
490--539 |
490--539 |
490--539 |
Elongation(%) |
10-30 |
10-30 |
10-30 |
Service temperature(°c) |
10-80 |
5-45 |
10-80 |
Main Characteristics
Electrical Resistance in Annealed Condition |
|||
Temp Coefficient of Electrical Resistance (a×10-6/°C) 20°C |
Operation Temperature °C |
Resistivity (uΩ/m,20°C) |
EMF VS Cu uV/°C(0~100°C) |
-0.7~40 |
0~100 |
0.44±4% |
≤2 |
Physical Characteristics (Reference Values) |
||||
Density g/cm3 |
Thermal conductivity (KJ/m.h°C) |
Tesile strength (N/mm2)Soft |
Elongation % |
Tesile strength (N/mm2) Hard |
8.4 |
40 |
390-535 |
6~15 |
≥585 |